Product name Wool content Yanr count Width(cm) Piece length(m) Weight(g/m) Remark
Twill coating 30-100% 40-50S/2 148-152 45-60 310-430
Serge 30-100% 45-100S/2 148-152 45-60 280-450 Can be double warp and single weft
Gabardine 30-100% 45-70S/2 148-152 45-60 310-420 Can be double warp and single weft, piece dyed,single gabardine
Fancy suiting 30-100% 22-70S/2 148-152 45-60 280-500
Valitin 30-100% 45-90S/2 148-152 45-60 210-340
Lady's dress cloth 30-100% 50-60S/2 148-152 45-60 230-380 Can be piece dyed
Satin drill 30-100% 42-80S/2 148-152 45-60 310-420 Can be double warp and single weft
Doeskin
Cavalry twill 20-100% 25-45S/2 148-152 45-60 400 upwards
Pure wool elastic fancy suiting 95-98% wool 40-60S/2 135-150 45-60 310-420  
LY2-5%
Wool blended elastic fancy suiting 30-80% wool 40-60S/2 135-150 45-60 290-420  
18-68% polyester
LY2%-4%
Wool blended elascti serge 30-80% wool 45-80S/2 135-150 45-60 280-420
18-68% polyester